Dentaurum Castorit All Speed 40 x 150 gms
Description
Castorit? All speed
High-expansion speed investment, individually controllablefor all alloys (except titanium).
Advantages:
casting ring can be placed into the furnace at finaltemperature (950 ?C / 1742 ?F) for speed preheatingor preheated in stages overnight
used for all alloy groups
the high overall expansion provides precision of fit
long working times and a very creamy mixing consistency
castings with extremely smooth surfaces ensure uniformquality and exact reproduction of the pattern
Norm:DIN EN ISO 15912
Type 1
Class 1, 2
Working time - 6 min
Preheating - consistent preheating,preheating with holdingtime, speed preheating
Preheating temperature - 70050 ?C / 1292742 ?F
Compression resistance - 91 MPa
Color - whitePackaging